ELECTROPHORETIC COATINGS | |||
---|---|---|---|
PROCESS | OPERATING CONDITIONS | APPLICATION | |
MASTER CLEAR EP 2000 | MASTER CLEAR EP 2000 MASTER EP 2000 DYE CIRCULATION ANODE CURING TEMPERATURE CURING TIME VOLTAGE | 250ml/l 20 – 40 ml/l CONTINOUS 316 SS 160 – 180 C 20 mins 40 – 60 V | Designed to produce clear as well as colored coatings. Very suitable for brass and jewellary items. Cathodic deposition type Acrylic based. Deposition up to 30 microns can be achieved. |
MASTER EP 2000 DYES (ACRYLIC) | MASTER EP 2000 DYES (ACRYLIC) | 20 – 40 ml/l | n tank dyes for electrophoretic coatings. Various colors available. |
MASTER EP 3000 POST DIP DY | MASTER EP 2000 POST DIP DYE TEMPERATURE | 80 – 100 ml/l 70 – 90 C | Post dip dyes for electrophoretic coatings. Very economical in use. Various colors available. |
MASTER EP 2000 PRE PASS NEUTRALIZER | MASTER EP 2000 PRE PASS NEUTRALIZER TEMPERATURE TIME | 50 – 75 g/l AmbienT 1 – 3 mins | Neutralizes the base coating prior to electrophoretic plating. Prevent cyanides to enter the EP 2000 bath. |